Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0356 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.986 g/cc
0.0356 lb/in³
Mixed
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works.
Density 0.986 g/cc
0.0356 lb/in³
Mixed
ITW Plexus Plexusâ„¢ MA1021 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low shrinkage.Information provided by Illinois Tool Works.
Density 0.986 g/cc
0.0356 lb/in³
Mixed
ITW Plexus Plexusâ„¢ MA1023 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works.
Density 0.986 g/cc
0.0356 lb/in³
Mixed
ITW Plexus Plexusâ„¢ MA1025 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, able to be used 1" thick.Information provided by Illinois Tool Works.
Density 0.985 - 0.995 g/cc
0.0356 - 0.0359 lb/in³
Solvay ANTAROX® LF 224 Surfactant
Chemical Name: ETHOXYLATED PROPOXYLATED ISODECYL ALCOHOLS CAS: 37251-67-5; 7732-18-5 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ANTAROX© LF-224 is used for t..
Density 0.985 g/cc
0.0356 lb/in³
Melt
Covestro Desmopan® DP 9659DU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro..
Density 0.985 g/cc
0.0356 lb/in³
Melt
Covestro Desmopan® DP 9662DU Polyurethane
Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro..
Density 0.985 g/cc
0.0356 lb/in³
ASTM D792, ISO 1183
DuPont™ Entira® ASSD100 Ionomer Resin
DuPont™ Entira™ AS SD100 is an extremely hygroscopic ionomer resin that is supplied as free flowing pellets. Entira™ AS SD100 is used to lower the static decay time and surface resistivity of LD..
Density 0.985 g/cc

@Temperature 15.0 °C
0.0356 lb/in³

@Temperature 59.0 °F
ISO 12185
ExxonMobil Solvesso™ 200 Aromatic Fluid
Appearance: Transparent - Slight Yellow LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil
Density 0.985 g/cc
0.0356 lb/in³
BASF 2-Phenylethylamine
Formula: C8H11NCAS: 64-04-0Description: 2-Phenylethylamine is a colorless to yellow liquid with an amine-like odor. Synonyms: Phenylethylamin, Benzolethanamin, PhenylethylamineApplications: Intermed..
Copyright © lookpolymers.com All Rights Reserved