Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.975 g/cc | 0.0352 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 9009 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 0.974 g/cc | 0.0352 lb/in³ | ASTM D792-91 |
Multibase Multi-Pro® 1010 T Black 10% Talc Content Polypropylene PPH talc filled compound suitable for containers and wash-tubs requiring elevated stiffness and improved cycle times.Data provided by Multibase. |
|||
Density | 0.975 g/cc | 0.0352 lb/in³ | ASTM D792 |
Global V-1160 High Density Polyethylene, Injection Molding Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containers, bottlesMeets FDA requirements as listed in.. |
|||
Density | 0.974 g/cc | 0.0352 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON MX12407C PP LNP* STAT-KON* MX12407C is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Density | 0.975 g/cc | 0.0352 lb/in³ | ASTM D792-ISO 1183 |
DuPont Elvax® 150W Ethylene Vinyl Acetate DuPont™ Elvax® 150W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p.. |
|||
Density | 0.973 g/cc @Temperature 40.0 °C |
0.0352 lb/in³ @Temperature 104 °F |
|
BASF PolyTHF® 2000 Polyether Description: PolyTHF 2000 is a colorless, odorless waxy substance. It is sparingly soluble in water and soluble organic solvents.Applications: Intermediate used in the production of: Synthesis of el.. |