Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.9215 g/cc | 0.03329 lb/in³ | ASTM D1505 |
Westlake EC479AA Low Density Polyethylene WESTLAKE low-density polyethylene EC479 is recommended for use in the boardstock coating industry. This resin has low neck-in, good heat sealing properties, and good drawdown characteristics.Applica.. |
|||
Density | 0.9215 g/cc | 0.03329 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2070G Linear Low Density Polyethylene High strength in food packaging applications Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Density | 0.9215 g/cc | 0.03329 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2070G Linear Low Density Polyethylene High strength in food packaging applications Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Density | 0.9215 g/cc | 0.03329 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2077G Linear Low Density Polyethylene Fast processing on narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Density | 0.9215 g/cc | 0.03329 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2077G Linear Low Density Polyethylene Fast processing on narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |