Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.9180 g/cc | 0.03316 lb/in³ | ExxonMobil Method |
ExxonMobil LL 3003.32 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Density | 0.9180 g/cc | 0.03316 lb/in³ | ExxonMobil Method |
ExxonMobil LL 3003.39 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Density | 0.9178 g/cc | 0.03316 lb/in³ | ASTM D792 |
Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-1003 NT 7 is an ethylene-hexene-1 copolymer, design.. |
|||
Density | 0.9178 g/cc | 0.03316 lb/in³ | ASTM D792 |
Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-1003 NT 7 is an ethylene-hexene-1 copolymer, design.. |
|||
Density | 0.9178 g/cc | 0.03316 lb/in³ | ASTM D792 |
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-7002 NT 7 is an ethylene-hexene-1 copolymer, design.. |
|||
Density | 0.9178 g/cc | 0.03316 lb/in³ | ASTM D792 |
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-7002 NT 7 is an ethylene-hexene-1 copolymer, design.. |