Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0320 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0320 g/cc
0.00116 lb/in³
Pyrotek G-2 Fiber Seal Pre-cut Gasket
A black, inexpensive material. Suitable for reusable gaskets.Information provided by Pyrotek.
Density 0.0320 g/cc
0.00116 lb/in³
Pyrotek G-2 Low-Temperature Felt
An inexpensive tough material.Dimensions610 mm x 30.5 m 25 mm thickApplicationsHigh-temperature gasketsInformation provided by Pyrotek.
Density 0.0320 g/cc
0.00116 lb/in³
Expectation from Single Pass Expansion
NOVA Chemicals Arcel 730 LV Resin 70% Polystyrene/30% Polyethylene
ARCEL advanced foam resin consists of polystyrene and polyethylene. ARCEL resin providesl toughness, flexibility and durability in a lightweight foam.The strength and flexibility of ARCEL resin crea..
Density 0.0320 g/cc
0.00116 lb/in³
core density
Ultracor® UCF-51-3/8-2.0 Honeycomb Core Material
Construction: ±45° XN50. Fiber: Carbon XN50. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures.  It is expected that it will be use..
Density 0.0320 g/cc
0.00116 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Plastazote® LD32CN Conductive Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0320 g/cc
0.00116 lb/in³
Hexcel® HexWeb® HRH-10 - 3/8 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Density 0.0320 g/cc
0.00116 lb/in³
Hexcel® HexWeb® HRH-36 - 3/16 - 2.0 Para-Aramid/Phenolic Core
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low..
Density 0.0320 g/cc
0.00116 lb/in³
Hexcel® HexWeb® HRH-36/OX - 3/16 - 2.0 Para-Aramid/Phenolic Core
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low..
Density 0.0320 g/cc
0.00116 lb/in³
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 2.0 Aramid Honeycomb
Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod..
Density 0.0320 g/cc
0.00116 lb/in³
Nominal
Hexcel® HexWeb® CR III 3/16-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Density 0.0320 g/cc
0.00116 lb/in³
Hexcel® HexWeb® HRH-10 - 1/2 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Density 0.0320 g/cc
0.00116 lb/in³
Hexcel® HexWeb® HRH-10 - 1/4 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Density 0.0320 g/cc
0.00116 lb/in³
Hexcel® HexWeb® HRH-10 - 3/16 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Density 0.0320 g/cc
0.00116 lb/in³
Free Rise Density (Cured)
Dow BETAFOAM™ 89100/89120
BETAFOAM™ 89100/89120 is a low-density, all-water blown rigid polyurethane foam. The components were engineered to produce a foam for providing barrier protection against airborne noise. Foam is ..
Density 0.0320 g/cc
0.00116 lb/in³
foam with adhesive; ASTM D3574
3M 4314 Single-Coated Foam Tape
3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast..
Density 0.0320 g/cc
0.00116 lb/in³
ASTM D3574
3M 4317 Foam Tape
Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio..
Density 0.0320 g/cc
0.00116 lb/in³
foam with adhesive; ASTM D3574
3M 4317 Single-Coated Foam Tape
3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast..
Density 0.0320 g/cc
0.00116 lb/in³
ASTM D3574
3M 4318 Foam Tape
Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio..
Density 0.0320 g/cc
0.00116 lb/in³
foam with adhesive; ASTM D3574
3M 4318 Single-Coated Foam Tape
3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast..
Density 0.0320 g/cc
0.00116 lb/in³
Free Rise Density, 3% H<sub>2</sub>O
ACC EP LS EPI Engineered Polymers Leak Stop MDI
EP LS, “Powered by Reactamine® Technology”, is a special MDI prepolymer designed to be pumped into voids or walls. EP LS reacts with water to create a shaving cream-like foam. This foam will soli..
Density 0.0320 g/cc
0.00116 lb/in³
ASTM D3574
3M 4314 Foam Tape
Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio..
Copyright © lookpolymers.com All Rights Reserved