Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.740 g/cc | 0.0267 lb/in³ | |
DuPont™ Nomex® N196 Paper, 15 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Density | 0.740 g/cc | 0.0267 lb/in³ | |
DuPont™ Nomex® N196 Paper, 3 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Density | 0.738 - 0.743 g/cc | 0.0267 - 0.0268 lb/in³ | BRCP 4843 |
ExxonMobil Nonene Olefin CAS Number: 68526-55-6Appearance: Clear, free of suspended matterInformation provided by ExxonMobil |
|||
Density | 0.740 g/cc | 0.0267 lb/in³ | |
BASF Butylamine Formula: C4H11NCAS: 109-73-9Description: Butylamine is a colorless liquid with an amine-like odor. It is miscible with water in all proportions.Synonyms: n-Butylamine, 1-Butanamine, Monobutylamin, .. |
|||
Density | 0.740 g/cc | 0.0267 lb/in³ | |
BASF Dipropylamine Formula: C6H |