Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Engineered Syntactic Systems AZ-40 Deep Water Syntactic Foam Syntactic foams are a combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having high c.. |
|||
Density | 0.609 - 0.673 g/cc | 0.0220 - 0.0243 lb/in³ | |
Engineered Syntactic Systems HZ-40 Deep Water Syntactic Foam Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having.. |