Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.560 - 0.580 g/cc | 0.0202 - 0.0210 lb/in³ | |
Sibur PVC S-5868-PZ Suspension Polyvinyl Chloride (PVC) For production of films and volume polymer containers for packing of food products and goods of public use. |
|||
Density | 0.560 g/cc | 0.0202 lb/in³ | ASTM D792 |
Covestro Baydur® 730 IBS Polyurethane Structural Foam RIM, Density 35 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Density | 0.560 g/cc | 0.0202 lb/in³ | |
3M Cushion-Mount™ E1840H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Density | 0.560 g/cc | 0.0202 lb/in³ | |
3M Cushion-Mount™ E1860H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Density | 0.560 g/cc | 0.0202 lb/in³ | |
Henkel SynSpand 9899 Expanding Syntactic Film Very high expansion, closed cell expanding film designed for use as shop floor aid in closed mold processes. |