Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 0.0140 g/cc | >= 0.000506 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
Ineos Nova T443B Expandable Polystyrene A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us.. |
|||
Density | 0.0140 - 0.0300 g/cc | 0.000506 - 0.00108 lb/in³ | Final Product Density |
Iran Petrochemical (PCC) TPC - 221 HS Expandable Polystyrene TPC - 221 HSApplication: low to medium density blocksInformation provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.0140 - 0.0250 g/cc | 0.000506 - 0.000903 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 255E Expandable Polystyrene General: Pentfoam 255E is a self extinguishing grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast expansion rate and short pressure.. |
|||
Density | 0.0140 - 0.0250 g/cc | 0.000506 - 0.000903 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 291L Expandable Polystyrene General: Pentfoam 291L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application.. |
|||
Density | 0.0140 - 0.0150 g/cc | 0.000506 - 0.000542 lb/in³ | |
IRPC Polimaxx Pentfoam 321F Expandable Polystyrene General: Pentfoam 321F is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine and convent.. |
|||
Density | 0.0140 - 0.0150 g/cc | 0.000506 - 0.000542 lb/in³ | |
IRPC Polimaxx Pentfoam 355E Expandable Polystyrene GENERAL: PENTFOAM "355E" IS A SELF EXTINGUISHING (SE) GRADE EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST EXPANSION RATE AND S.. |
|||
Density | 0.0140 g/cc | 0.000506 lb/in³ | 1.2 minute residence time pre-expander |
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ.. |
|||
Density | 0.0140 - 0.0180 g/cc | 0.000506 - 0.000650 lb/in³ | sheet density |
Zotefoams Plastazote® LD14IC Low Density Polyethylene Foam, Intermediate Cell Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0140 - 0.0190 g/cc | 0.000506 - 0.000686 lb/in³ | sheet density |
Zotefoams Plastazote® LD15FM Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0140 - 0.0180 g/cc | 0.000506 - 0.000650 lb/in³ | sheet density |
Zotefoams Plastazote® LD15IC Low Density Polyethylene Foam, Intermediate Cell Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0140 - 0.0190 g/cc | 0.000506 - 0.000686 lb/in³ | sheet density |
Zotefoams Plastazote® LD15FMSV Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0140 - 0.0180 g/cc | 0.000506 - 0.000650 lb/in³ | sheet density |
Zotefoams Plastazote® MP15 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0140 - 0.0180 g/cc | 0.000506 - 0.000650 lb/in³ | sheet density |
Zotefoams Plastazote® MP15FR Metallocene Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0140 - 0.110 g/cc | 0.000506 - 0.00397 lb/in³ | |
BASF Styropor® BFL 222 EPS Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c.. |
|||
Density | 0.0140 - 0.0480 g/cc | 0.000506 - 0.00173 lb/in³ | |
BASF Styropor® BF 222 EPS Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv.. |
|||
Density | <= 0.0140 g/cc | <= 0.000506 lb/in³ | TMA |
Akzo Nobel Expancel® 091 DU 140 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0140 g/cc | <= 0.000506 lb/in³ | TMA |
Akzo Nobel Expancel® 092 DU 120 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0140 - 0.0180 g/cc | 0.000506 - 0.000650 lb/in³ | sheet density |
Zotefoams Plastazote® LD15 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |