Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.380 - 0.420 g/cc | 0.0137 - 0.0152 lb/in³ | ASTM D792 |
Microcell Composite Company CELLOMER® S-2140 SBS Rubber Foam CELLOMER® FOAM is non-toxic, contains no heavy metal, PVC-free, chloride-free, light weight, superior-grip in wet & dry, high elasticity & resilience. Can be 100% recycled.Information provided by.. |
|||
Density | 0.380 g/cc | 0.0137 lb/in³ | Typical, 3M QCM 14.24.6 |
3M HGS4000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |
|||
Density | 0.380 g/cc | 0.0137 lb/in³ | |
3M S38 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.380 g/cc | 0.0137 lb/in³ | |
3M S38HS Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.380 g/cc | 0.0137 lb/in³ | |
3M S38XHS Glass Bubbles 3M™ Glass Bubbles S38XHS have a density of .38 g/cc and an isostatic crush strength of 5500 psi with a minimum survival of 90% as compared to S38HS, which has a target 90% survival of 5500 psi. Lik.. |
|||
Density | 0.380 g/cc | 0.0137 lb/in³ | Typical, 3M QCM 14.24.6 |
3M HGS5000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |