Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.150 g/cc | 0.00542 lb/in³ | at 0.06 MPa |
Zircar Ceramics APA-2 Alumina Paper ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-2 is a flexible un-bonded sheet that contains no organic binder. Applications include thermal insulation in low .. |
|||
Density | 0.150 - 0.200 g/cc | 0.00542 - 0.00723 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 F-7142 EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.150 g/cc | 0.00542 lb/in³ | |
3M K15 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.150 g/cc | 0.00542 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® T90.150 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |
|||
Density | 0.150 g/cc | 0.00542 lb/in³ | |
3M S15 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.150 - 0.190 g/cc | 0.00542 - 0.00686 lb/in³ | ISO 845-88 |
Eurofoam Porocell 251 BG NBR/PVC Foam Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurof.. |
|||
Density | 0.150 g/cc | 0.00542 lb/in³ | |
Mo-Sci Corporation GL-0237 Hollow Glass Spheres Appearance: Hollow microspheres with white color in powder form.Applications: GL-0237 is a new, low cost, light weight, hollow glass extender for liquid resin systems offering low cost per unit volu.. |