Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Pyrotek M-8 Fiber Seal Pre-cut Gasket Contains no binders and is not changed by exposure to high temperatures.Information provided by Pyrotek. |
|||
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Sharadaa Ceramics And Bulk Fiber Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Sharadaa Ceramics Blankets Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Zircar Refractory Composites RSBL-SOL8 Silica-Magnesia Blanket ZIRCAR Refractory Composites, Inc. insulating blankets are non woven, inorganic, fiber-based products that contain no asbestos. They are engineered for use as thermal barrier materials in high tempe.. |
|||
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Zircar Refractory Composites ASPA-2 Alumina-Silica Fiber Paper ASPA-2 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c.. |
|||
Density | 0.128 g/cc | 0.00462 lb/in³ | |
Pyrotek M-8 Fiberseal Blanket Stitched with high-temperature fibers. Contains no binders. Not changed by exposure to high temperatures.Dimensions610 mm x 7.6 m25 mm thickApplicationsHigh-temperature gaskets Furnace linings Gen.. |