PRODUCT NO. Manufacturer Trade Name
Plastcom SLOVALEN PH 49 GF 50 Polypropylene Homopolymer, 50% Glass Fiber Plastcom spol. s r.o. SLOVALEN
Plastcom SLOVALEN PH 69 GF 45 PP, 45% glass fibre Plastcom spol. s r.o. SLOVALEN
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced PlastiComp Complēt®
RTP Company VLF 80109 CC Polypropylene (PP), Long Glass Fiber - Chemically Coupled RTP Company VLF
MTI ThermoStran® PP-50G Long Glass Fiber Compound MTI Thermoplastic Composites, Division of Montsinger Technologies, Inc. (MTI) ThermoStran®
LATI Latene® AG7H2 G/50 PP Homopolymer, 50% Glass Fiber Reinforced, Heat Stabilized LATI Latene®
Techmer ES HiFill® PP LGF50 CC NAT 12mm 50% Glass Filled Techmer ES HiFill®
Techmer ES HiFill® PP GF50 CC HF BK 50% Glass Filled Techmer ES HiFill®
A. Schulman POLYFORT™ FPP 3710 Glass Filled Homopolymer Polypropylene
A. Schulman POLYFORT™ FPP 3710 Glass Filled Homopolymer Polypropylene
Polyram Polytron P50B03 Copolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber Polyram Polytron
Polyram Polytron P50B07 Polypropylene, 50% Long Glass Fiber, UV Stabilized Polyram Polytron
Polyram Polytron P50B11 Homopolymer Polypropylene, Chemically Coupled 50% LGF Polyram Polytron
Polyram Polytron P50N01 Homopolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber Polyram Polytron
Polyram Polytron P50N07 Polypropylene, 50% Long Glass Fiber, UV Stabilized Polyram Polytron
A. Schulman POLYFORT™ FPP 3710 Glass Filled Homopolymer Polypropylene
RTP Company RTP 109 Polypropylene (PP), Glass Fiber RTP Company
A. Schulman POLYFORT™ FPP 3710 Glass Filled Homopolymer Polypropylene
A. Schulman POLYFORT™ FPP 3710 Glass Filled Homopolymer Polypropylene A. Schulman, Inc. POLYFORT™
Polyram RamOfin PPH300G9 Polypropylene, 45% Glass Fiber Polyram
RTP Company RTP 109 CC Polypropylene (PP), Glass Fiber - Chemically Coupled RTP Company
Cossa Polimeri ESTAPROP H 05100 GFC Polypropylene, 50% Glass Filled Cossa Polimeri S.r.L. ESTAPROP
Entec Hypro™ PPC-GF30 Natural Impact Polypropylene, 30% Glass Reinforced Entec Engineered Resins Hypro™
Eurotec® Tecolen® CP10 GR50 NL PPCP, 50% glass fiber reinforced, natural Eurotec Tecolen®
Bond Laminates TEPEX® dynalite 104-RG600(x)/47% Roving Glass – PP Consolidated Composite Laminate Bond Laminates TEPEX® dynalite
Celanese Celstran® PP-GF50-02- Natural PP, 50% Glass Reinforced Celanese Corporation CELSTRAN
Celanese Celstran® PP-GF50-02-Black PP, 50% Glass Reinforced Celanese Corporation CELSTRAN
Celanese Celstran® PP-GF50-03-Black PP, 50% Glass Reinforced Celanese Corporation CELSTRAN
Celanese Celstran® PP-GF50-0403 P10 PP, 50% Glass Reinforced Celanese Corporation CELSTRAN
Celanese Celstran® PP-GF50-0403 P10/10 PP, 50% Glass Reinforced Celanese Corporation CELSTRAN
Celanese Celstran® PP-GF50-0405P10/10 PP, 50% Glass Reinforced Celanese Corporation CELSTRAN
Celanese Celstran® PP-GF50-0453 P10/10 PP, 50% Glass Reinforced Celanese Corporation CELSTRAN
Celanese Celstran® PP-GF50-0455 P10/10 PP, 50% Glass Reinforced Celanese Corporation CELSTRAN
Asahi Kasei Thermylene® P7-45FG-0790 45% Glass Fiber Reinforced, Heat Stabilized Asahi Kasei Thermylene®
Celanese Celstran® PP-GF50-10 PP, 50% Glass Reinforced Celanese Corporation CELSTRAN
Celanese Celstran® PP-GF50-02 PP, 50% Glass Reinforced Celanese Corporation Celstran®
Celanese Celstran® PP-GF50-03 PP, 50% Glass Reinforced Celanese Corporation Celstran®
Celanese Celstran® PP-GF50-0403P10/10 PP, 50% Glass Reinforced Celanese Corporation Celstran®
Celanese Celstran® PP-GF50-0453P10/10 PP, 50% Glass Reinforced Celanese Corporation Celstran®
Celanese Celstran® PP-GF50-0455P10/10 PP, 50% Glass Reinforced Celanese Corporation Celstran®
Celanese Celstran® PP-GF50-0458 P10/10 PP, 50% Glass Reinforced Celanese Corporation Celstran®
Celanese Celstran® PP-GF50-BV337 PP, 50% Glass Reinforced Celanese Corporation Celstran®
A. Schulman POLYFORT™ FPP 3710 Glass Filled Homopolymer Polypropylene
Polyram Polytron P50B01 Homopolymer Polypropylene, Chemically Coupled 50% LGF Polyram Polytron
Celanese Celstran® +PP-GF45-05X551/1X PP, 45% Glass Reinforced Celanese Corporation CELSTRAN
Overview of materials for Polypropylene, Long Glass Fiber 50%