Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Asia Pacific) SABIC Innovative Plastics (GE Plastics) LNP LUBRICOMP
SABIC Innovative Plastics LNP Thermocomp KF002A Acetal Homopolymer SABIC Innovative Plastics (GE Plastics) LNP THERMOCOMP
SABIC Innovative Plastics LNP Thermocomp KF002A Acetal Homopolymer (Asia Pacific) SABIC Innovative Plastics (GE Plastics) LNP THERMOCOMP
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly SABIC Innovative Plastics (GE Plastics) LNP THERMOCOMP
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific) SABIC Innovative Plastics (GE Plastics) LNP THERMOCOMP
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly (Asia Pacific) SABIC Innovative Plastics (GE Plastics) LNP THERMOCOMP
SABIC Innovative Plastics LNP THERMOCOMP KF004A Acetal Homopolymer SABIC Innovative Plastics (GE Plastics) LNP THERMOCOMP
SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopoly (Asia Pacific) SABIC Innovative Plastics (GE Plastics) LNP THERMOCOMP
SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopolymer SABIC Innovative Plastics (GE Plastics) LNP THERMOCOMP
SABIC Innovative Plastics LNP Lubricomp KFI12A Acetal Homopolymer SABIC Innovative Plastics (GE Plastics) LNP LUBRICOMP
DuPont Performance Polymers Delrin® 510GR NC000 Acetal (POM)  (Unverified Data**) DuPont Performance Polymers Delrin®
DuPont Performance Polymers Delrin® 525GR NC000 Acetal (POM)  (Unverified Data**) DuPont Performance Polymers Delrin®
DuPont Performance Polymers Delrin® 570 NC000 Acetal (POM)  (Unverified Data**) DuPont Performance Polymers Delrin®
DuPont Performance Polymers Delrin® 577 BK000 Acetal (POM)  (Unverified Data**) DuPont Performance Polymers Delrin®
Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM) Ensinger Delrin®
DuPont Performance Polymers Delrin® FG570 NC000 Acetal Homopolymer DuPont Performance Polymers Delrin®
Asahi Kasei Tenac® GA520 Homopolymer Acetal Resin Asahi Kasei Tenac®
Asahi Kasei Tenac® GN705 Homopolymer Acetal Resin Asahi Kasei Tenac®
Asahi Kasei Tenac® GA510 Homopolymer Acetal Resin Asahi Kasei Tenac®
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer  (Unverified Data**)
RTP Company RTP 801 DEL Acetal (POM) Glass Fiber - Homopolymer RTP Company
RTP Company RTP 802 SI 2 DEL Acetal (POM), Glass Fiber - Silicone Lubricated - Homopolymer RTP Company
RTP Company RTP 803 DEL Acetal (POM), Glass Fiber - Homopolymer RTP Company
RTP Company RTP 803 Z DEL Acetal (POM) Glass Fiber - FDA Compliant Ingredients - Homopolymer RTP Company
DuPont Performance Polymers Delrin® 570 NC000 Acetal Homopolymer  (Unverified Data**)